MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Go Yen Chemical GY-FR-CW Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: It is the flame retardant for plastic such as PVC, PP, PE, ABS, PS, etc

Applications:

  • GY-FR-CW is a good secondary plasticizer
  • It is the flame retardant for plastic such as PVC, PP, PE, ABS, PS, etc.
  • Applied in rubber industry.
  • GY-FR-CW can be used in paint ,coating adhesives
  • As flame retardant for textile.
  • With the high chlorine content and good compatibility with base oil ,GY-FR-CW also serves as a good extreme pressure additive in lubricant for metal working liquid.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 - 1.27 g/cc
Viscosity 11 - 16 cP
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.10mg KOH/g
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl 50 - 52 %
 
Descriptive Properties
AppearanceLiquid
Color<120APHA
 Light colored
Thermal Stability<0.2%HCL 4 hrs 175°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN084 / 266392

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.