Petrothene XL07420B is a colorable, non-halogenated, flame retardant compound crosslinkable via continuous vulcanization (C.V.). Petrothene XL07420B is selected for use in ISO 125 °C thin wall automotive wire & cable applications. Applications: Wire & CableInformation provided by LyondellBasell. |