MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Evonik VESTODUR® GF12-FR3 orange E20039 Polybutylene Terephthalate  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled

Material Notes: Glass fiber-reinforced polybutylene terephthalate compound with non-migrating and non-corrosive flame retardant. VESTODUR® GF12-FR3 orange E20039 is a glass fiber-reinforced (12.5%), self-extinguishing poly­butylene terephthalate (PBT) compound with an orange color. The compound is suitable for manufacturing parts subjected to high mechanical and thermal loads. Test bars made of this compound are rated self-extinguishing according to UL94 by Underwriters Laboratories Inc. The incorporated flame retardant is non-migrating and has no corrosive effects on metal inserts or neighboring metal parts. Therefore VESTODUR® GF12-FR3 orange E20039 is distin­guished for moldings in the electrical and electronical industry. Laser marking with high contrasts is possible. VESTODUR® GF12-FR3 is supplied as cylindrical pellets in polyethylene packaging. Pigmentation may affect values.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 90.0 MPa13100 psiISO 527
Tensile Strength 90.0 MPa13100 psiISO 527
Elongation at Break 2.5 %2.5 %ISO 527
Tensile Modulus 6.20 GPa899 ksiISO 527
Charpy Impact Unnotched 3.70 J/cm²
@Temperature 23.0 °C
17.6 ft-lb/in²
@Temperature 73.4 °F
Complete Break; ISO 179/1eU
Charpy Impact, Notched 0.450 J/cm²
@Temperature 23.0 °C
2.14 ft-lb/in²
@Temperature 73.4 °F
Complete Break; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Flammability Test  5.0
@Thickness 0.400 mm
5.0
@Thickness 0.0157 in
IEC 60695-11-10
 5.0
@Thickness 1.60 mm
5.0
@Thickness 0.0630 in
IEC 60695-11-10
 5.0
@Thickness 3.20 mm
5.0
@Thickness 0.126 in
IEC 60695-11-10

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK882 / 243089

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.