MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akro-Plastic Akromid® A3 GF 15 black (2425) PA 6.6 Dry, 15% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: Description: AKROMID A3 GF 15 black (2425) is a 15% glass fiber reinforced polyamide 6.6 with medium stiffness and strength. Applications are mainly component in mechanical engineering and in the automotive industry.

Features:

  • Good Stiffness
  • Medium Strength
Uses:
  • Automotive Applications
  • Engineering Parts

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccISO 1183
Filler Content 15 %ISO 1172
Moisture Absorption 2.5 - 2.7 %
@Temperature 70.0 °C
Humidity, 62% RH; ISO 1110
Water Absorption at Saturation 6.7 - 7.3 %ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.014 cm/cmISO 294-4
Spiral Flow 99.0 cmCross section: 7 mm x 3.5 mm
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 200 MPaHB 961/30; ISO 2039-1
Tensile Strength at Break 140 MPa5 [mm/min]; ISO 527-2
Elongation at Break 3.5 %5 [mm/min]; ISO 527-2
Tensile Modulus 6400 MPa1 [mm/min]; ISO 527-2
Flexural Strength 200 MPa2 [mm/min]; ISO 178
Flexural Modulus 6100 MPa2 [mm/min]; ISO 178
Charpy Impact Unnotched 43.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 45.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 7.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 34.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Melting Point 262 °CDIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi) 260 °CUnannealed; ISO 75/B
Deflection Temperature at 1.8 MPa (264 psi) 245 °CUnannealed; ISO 75/A
Flammability, UL94 HB
@Thickness 1.60 mm
Glow Wire Flammability Index 650 °C
@Thickness 1.60 mm
IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled
Overview of materials for Nylon 66, Unreinforced
Domo Technyl® C216V15 15% Glass Filled Nylon 6
Overview of materials for Nylon 66, 10% Glass Fiber Filled
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Conditioned, 15% Glass Filled

PAKRO177 / 182764

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.