Moplen RP390T is a nucleated random copolymer used for injection molding. Moplen RP390T offers a very good flowability and an excellent transparency and organoleptic performance. Moplen RP390T is typically used in the production of thin walled packaging with high transparency and high requirements for organoleptic properties. In multilayer barrier systems, processors have found that it provides good adhesion with the inner barrier layer, without impacting the overall transparency and process ability. Moplen RP390T has a superior aesthetic appearance and can be processed at significantly lower temperatures, enabling convertors to generate energy savings and improved productivity due to reduced cycle times. Moplen RP390T is a development grade. Applications: Clear Containers, House wares.Information provided by LyondellBasell. |