MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® OG142 UV Cure Optical Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Material Description: A single component, UV curable epoxy, designed for adhesive, sealing, and encapsulating applications found in semiconductor, electro-optics, fiber optics, medical, and scientific/OEM industries. It is a high Tg epoxy, ideal for LCD and OLED applications.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/cc
Viscosity 9000 - 15000 cP
@Temperature 23.0 °C
20 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 86
Tensile Modulus 222000 psiStorage
Shear Strength >= 1360 psiDie
 
Thermal PropertiesOriginal ValueComments
CTE, linear 58.0 µm/m-°CBelow Tg
 156 µm/m-°CAbove Tg
Maximum Service Temperature, Air 200 °CContinuous
 300 °CIntermittent
Minimum Service Temperature, Air -55.0 °CContinuous
 -55.0 °CIntermittent
Glass Transition Temp, Tg >= 95.0 °CPost-Cure Dynamic Scan 20200°C; Ramp -40200°C @ 20°C/Min
Decomposition Temperature 421 °CDegradation Temperature
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.5692
@Wavelength 589 nm
Transmission, Visible >= 92 %
@Wavelength 440 - 620 nm
Spectral
 >= 97 %
@Wavelength 660 - 1640 nm
Spectral
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 25.0 °C
 
Descriptive Properties
ColorCloudy/Colorlessbefore cure
ConsistencyPourable liquid
Number of ComponentsSingle
Weight Loss0.2%200°C
 0.49%250°C
 1.06%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® B9021-1 Epoxy Paste
MarkeTech Yttrium Vanadate (YVO4) Fiber Optic Crystal
MarkeTech Rutile (TiO2) Fiber Optic Crystal
Epoxy Technology EPO-TEK® OG178 UV Cure Optical Epoxy
Borosilicate Glass

PPOXYT166 / 141205

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.