MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Trilliant™ HC HC5210-0020 RS Natural Polypropylene Homopolymer (PP Homopolymer)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Filler Content 20 %Unspecified
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 105ASTM D785
Tensile Strength, Yield 64.1 MPaType I, 51 mm/min; ASTM D638
Elongation at Break 10 %Type I, 51 mm/min; ASTM D638
Flexural Strength 90.3 MPaASTM D790
Flexural Modulus 3520 MPaASTM D790
Izod Impact, Notched 69.0 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
Izod Impact, Unnotched 310 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 157 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
ALL; UL 94
 
Compliance PropertiesOriginal ValueComments
FDA YesUnspecified Rating
 
Descriptive Properties
AppearanceNatural Color
FeaturesChemically Coupled
 Homopolymer
 Specialty Grade
Filler / ReinforcementGlass Fiber Reinforcement
FormsPellets
Generic MaterialPP Homopolymer
Generic NamePolypropylene Homopolymer (PP Homopolymer)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesDisposable Hospital Goods
 Hospital Goods
 Medical Device Housings
 Medical/Healthcare Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eagle Brass 521 Phosphor Bronze 8% C, 1/4 Hard
Phosphor bronze 8% Sn, UNS C52100
Eagle Brass 521 Phosphor Bronze 8% C, Extra Hard
Eagle Brass 521 Phosphor Bronze 8% C, Extra Spring
Eagle Brass 521 Phosphor Bronze 8% C, Hard

PH0POL1289 / 145858

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.