MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Erbslöh Aluminium DISPAL S236 Aluminum Alloy, Condition T6x
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes:

Information provided by PEAK Werkstoff GmbH, a part of Erbslöh Aluminium GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.69 - 2.97 g/cc0.0972 - 0.107 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers >= 210>= 210HV30
Tensile Strength at Break  >= 415 MPa
@Temperature 150 °C
>= 60200 psi
@Temperature 302 °F
 >= 480 MPa
@Temperature 20.0 °C
>= 69600 psi
@Temperature 68.0 °F
Tensile Strength, Yield  >= 351 MPa
@Temperature 150 °C
>= 50900 psi
@Temperature 302 °F
0.2% offset
 >= 410 MPa
@Temperature 20.0 °C
>= 59500 psi
@Temperature 68.0 °F
0.2% offset
Elongation at Break  >= 0.5 %
@Temperature 20.0 °C
>= 0.5 %
@Temperature 68.0 °F
 >= 0.6 %
@Temperature 150 °C
>= 0.6 %
@Temperature 302 °F
Modulus of Elasticity  >= 85.0 GPa
@Temperature 150 °C
>= 12300 ksi
@Temperature 302 °F
 >= 103 GPa
@Temperature 20.0 °C
>= 14900 ksi
@Temperature 68.0 °F
Fatigue Strength  123.3 MPa
@# of Cycles 5.00e+7 ,
Temperature 150 °C
17880 psi
@# of Cycles 5.00e+7 ,
Temperature 302 °F
P50% rotary bending value, σbW
 232.2 MPa
@# of Cycles 5.00e+7 ,
Temperature 20.0 °C
33680 psi
@# of Cycles 5.00e+7 ,
Temperature 68.0 °F
P50% rotary bending value, σbW
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000120 ohm-cm0.0000120 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  15.5 - 16.5 µm/m-°C
@Temperature 20.0 - 100 °C
8.61 - 9.17 µin/in-°F
@Temperature 68.0 - 212 °F
 16.2 - 17.2 µm/m-°C
@Temperature 20.0 - 200 °C
9.00 - 9.56 µin/in-°F
@Temperature 68.0 - 392 °F
 17.0 - 18.0 µm/m-°C
@Temperature 20.0 - 300 °C
9.44 - 10.0 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.740 - 0.780 J/g-°C0.177 - 0.186 BTU/lb-°F
Thermal Conductivity  84.0 W/m-K
@Temperature 30.0 °C
583 BTU-in/hr-ft²-°F
@Temperature 86.0 °F
T6(SB) Condition
 87.0 W/m-K
@Temperature 200 °C
604 BTU-in/hr-ft²-°F
@Temperature 392 °F
T6(SB) Condition
 87.0 W/m-K
@Temperature 100 °C
604 BTU-in/hr-ft²-°F
@Temperature 212 °F
T6(SB) Condition
 89.0 W/m-K
@Temperature 300 °C
618 BTU-in/hr-ft²-°F
@Temperature 572 °F
T6(SB) Condition
 91.0 W/m-K
@Temperature 400 °C
632 BTU-in/hr-ft²-°F
@Temperature 752 °F
T6(SB) Condition
Melting Point 523 - 796 °C973 - 1460 °F
Solidus 522.8 - 528.8 °C973.0 - 983.8 °F
Liquidus 789.6 - 795.6 °C1453 - 1464 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6061-T6; 6061-T651
Erbslöh Aluminium DISPAL S220 Aluminum Alloy, AlSi35, Condition O
Erbslöh Aluminium DISPAL S236 Aluminum Alloy, Condition T6(SB)
Erbslöh Aluminium DISPAL S236 Aluminum Alloy, Condition F
Erbslöh Aluminium DISPAL S256 Aluminum Alloy, Condition F

NPEAK04o / 192055

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.