MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Tefzel® HT-2181 Fluoropolymer Resin
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: DuPont™ Tefzel® HT-2181 fluoropolymer resin is a general-purpose resin available in translucent, 2.5-mm (0.1-in) pellets. Compared with other grades of Tefzel® , its most unique features are an intermediate flow rate and a balance of properties that make it suitable for a variety of processes and demanding end uses. Tefzel® HT-2181 and the other Tefzel® fluoropolymers are melt processible, modified copolymers of ethylene and tetrafluoroethylene. They are high-performance resins that can be processed at relatively high rates compared with other fluorocarbon resins. They are mechanically tough and offer an excellent balance of properties.

Tefzel® HT-2181 can perform successfully in applications where other thermoplastics are lacking in mechanical toughness, broad thermal capability, ability to meet difficult environmental conditions, or limited by fabricating problems.

Properly processed products made from neat Tefzel® HT-2181 are inert to most solvents and chemicals, hydrolytically stable, and weather-resistant. The recommended upper service temperature is 155°C (311°F); useful properties are retained at cryogenic ranges. The level and stability of dielectric properties are excellent, and the flame rating is V-0 by the UL94 method. Mechanical properties include outstanding impact strength, cut-through, and abrasion resistance. Statements, or data, regarding behavior in a flame situation are not intended to reflect hazards presented by this or any other material when under actual fire conditions.

Applications

Tefzel® HT-2181 is ideal for many end products, including electrical components, such as sleeving, coil forms, sockets, connectors, and switches; lab ware, such as tubing, valves, containers, and dishes; battery or instrument components that require chemical inertness; chemical service items, such as valve components, seal glands, pipe plugs, and corrugated tubing; and film.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Key Words: Ethylene Tetrafluoroethylene Copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.70 g/ccASTM D792
Bulk Density 1.30 g/cc
Water Absorption 0.0070 %24 hours; ASTM D570
Melt Flow 6.0 g/10 minASTM D3159
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 67ASTM D2240
Tensile Strength, Ultimate 40.0 MPaASTM D638
Elongation at Break 300 %ASTM D638
Flexural Modulus 1.0 GPaASTM D790
Izod Impact, Notched NBASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D257
Dielectric Constant 2.5 - 2.6
@Frequency 1e+6 Hz
ASTM D1531
Dielectric Strength 70.0 kV/mm
@Thickness 0.250 mm
ASTM D150
Dissipation Factor 0.0060
@Frequency 1e+6 Hz
ASTM D1531
Arc Resistance 122 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 131 µm/m-°C
@Temperature 0.000 - 100 °C
ASTM D696
Melting Point 255 - 280 °CASTM D3418
Maximum Service Temperature, Air 155 °C
Flammability, UL94 V-0
Oxygen Index 30 - 32 %ASTM D2863
 
Descriptive Properties
Chemical/Solvent ResistanceExcellent
Weather ResistanceExcellentYears unaffected in Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Tefzel® HT-2190 Fluoropolymer Resin
Chemours Tefzel® HT-2185 Fluoropolymer Resin
Chemours Tefzel® HT-2183 Fluoropolymer Resin
Chemours Tefzel® HT-2127 Fluoropolymer Resin
Chemours Tefzel® HT-2202 Fluoropolymer Resin

PDU9298 / 33365

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.