MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Pebax® Clear 300 Polyether Block Amide (PEBA)
Categories: Polymer; Thermoplastic; Polyether Block Amide (PEBA)

Material Notes: Pebax® Clear 300 combines high transparency level with the unique performance of Pebax®, thermoplastic elastomer made of flexible polyether and rigid polyamide.

Information provided by Arkema Group. Property data for dry samples, unless noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
Water Absorption 1.6 %Sim. to ISO 62
Moisture Absorption 0.700 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0040 cm/cmISO 294-4 2577
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 53
@Time 15.0 sec
ISO 868
Tensile Strength, Yield 13.0 MPaConditioned; ISO 527-1/-2
Elongation at Break >= 50 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 20 %Conditioned; ISO 527-1/-2
Tensile Modulus 250 MPaConditioned; ISO 527-1/-2
Flexural Modulus 212 MPaConditioned 15 days at 23°C - 50% RH; ISO178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched NB
@Temperature -30.0 °C
ISO 179/1eA
 NB
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 °C10°C/min; ISO 11357-1/-3
Vicat Softening Point 119 °C50°C/h 50N; ISO 306
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Transparent, but thickness not reported; ISO 13468-1 -2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 °CInjection Molding; ISO 294
Mold Temperature 23.0 °CInjection Molding; ISO 10724

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Pebax® Clear 400 Polyether Block Amide (PEBA)
Arkema Pebax® 4533 SP 01 TPA
Arkema Pebax® 6333 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® MV 1074 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® 5533 SN 70 BLACK Polyether Block Amide (PEBA) (Dry)

PZARKG701 / 142496

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.