MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Ultramid® 8231G HS BK-102 14% Glass Filled PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled

Material Notes: Ultramid 8231G HS BK-102 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffness and heat deflection temperature. The heat stabilizer system extends the properties at elevated temperatures. It also has excellent chemical resistance to greases, oils and hydrocarbons.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccdry; ISO 1183
Water Absorption 1.4 %24 hour; ISO Test
 8.1 %beginning dry; ISO 62
Moisture Absorption at Equilibrium 2.3 %beginning dry (23°C/50% R.H.); ISO 62
Relative Viscosity 2.6 cPISO Test; 96 % SAV
Viscosity Measurement 50Formic Acid
Linear Mold Shrinkage 0.0050 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPa0.2 in/min; ASTM Test
 30.0 MPa
@Temperature 80.0 °C
ISO Data
 30.0 MPa
@Temperature 80.0 °C
ASTM Test
 40.0 MPa
@Temperature 120 °C
ASTM Test
 40.0 MPa
@Temperature 120 °C
ISO Data
 150 MPa
@Temperature -40.0 °C
ISO Data
 150 MPa
@Temperature -40.0 °C
ASTM Test
Tensile Strength, Ultimate 60.0 MPa5mm/min; ISO 527
Elongation at Break 20 %5mm/min; ISO 527
 20 %0.2 in/min; ASTM Test
 3.0 %
@Temperature -40.0 °C
ASTM Test
 3.0 %
@Temperature -40.0 °C
ISO Data
 9.0 %
@Temperature 120 °C
ISO Data
 9.0 %
@Temperature 120 °C
ASTM Test
 15 %
@Temperature 80.0 °C
ASTM Test
 15 %
@Temperature 80.0 °C
ISO Data
Tensile Modulus 3100 MPa1mm/min; ISO 527
 1800 MPa
@Temperature 120 °C
ISO Data
 2300 MPa
@Temperature 80.0 °C
ISO Data
 6900 MPa
@Temperature -40.0 °C
ISO Data
Flexural Strength 65.0 MPaISO Data
Flexural Modulus 2210 MPaISO Data
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °C10 K/min
 220 °CASTM Test
 
Processing PropertiesOriginal ValueComments
Melt Temperature 275 °CInjection molding
Mold Temperature 95.0 °CInjection molding
 
Descriptive Properties
ColorBK-102
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
Special characteristicHeat stabilized or stable to heat
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8231G HS BK-102 14% Glass Filled PA6 (Dry)
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry)
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Conditioned)
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Conditioned)
BASF Ultramid® 8231G HS BK-106 14% Glass Filled PA6 (Dry)

PBASF9154 / 84918

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.