MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nouryon Trigonox EHP-W40S Di(2-ethylhexyl) peroxydicarbonate
Categories: Other Engineering Material

Material Notes: Initiator (40% frozen emulsion in water) for (co)polymerization of vinyl chloride and vinylidene chloride.

CAS number: 16111-62-9

EINECS/ELINCS No: 240-282-4

Applications: Polymerization of vinyl chloride: emulsions and suspension of peroxides are more and more accepted in the market. Why to use aqueous emulsions or suspensions? Safety reasons, Solvent free: no contamination of the VCM recycle stream, enhancement of PVC purity, easily to use (pumpable) in ‘closed reactor technology’ and easily to dilute with water. Trigonox EHP-W40S can be diluted with water provided agitation is used to prevent possible phase separation. To melt the solid Trigonox EHP-W40S dilution with water is the most elegant way. Short term stability of Trigonox EHP-W40S or the dilution is sufficient enough to allow handling at temperatures up to 5°C for a short time. Trigonox EHP-W40S is used for the suspension polymerization of vinyl chloride in the temperature range 40-65°C. In practice, Trigonox EHP-W40S is often combined with other peroxides to increase reactor efficiency.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.330 g/cc0.0119 lb/in³
Half-life  0.100
@Temperature 83.0 °C
0.100
@Temperature 181 °F
[hr]
 1.00
@Temperature 64.0 °C
1.00
@Temperature 147 °F
[hr]
 10.0
@Temperature 47.0 °C
10.0
@Temperature 117 °F
[hr]
Viscosity 100 cP
@Temperature 0.000 °C
100 cP
@Temperature 32.0 °F
Molecular Weight 346.5 g/mol346.5 g/mol
Storage Temperature -25.0 - -15.0 °C-13.0 - 5.00 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point -1.00 - 0.000 °C30.2 - 32.0 °F
Decomposition Temperature 5.00 °C41.0 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceWhite flakes
Content500 mg/kgInorganic + organic hydrolysable chloride
Content (%)4.62Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1183 / 286706

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.