Introduction IROGRAN A 92 E 4670 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion/injection molding product range and offers a specially designed, flexible material with a broad processing window. Performance Features: - High oil resistance
- High production rate
- Good melt flow
- Easy coloring
- Complies with FDA CFR 175.105 /177.2600
Applications: - Cable jacketing
- Tubing
- Technical extrusion.
|