MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman BMC T40(25)-XHS Die Casting Replacement Grade Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: BMC T40(25)-XHS is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical properties and ability to maintain machined tolerances in a molding part it is used widely as a direct replacement for die castings. T40(25)-XHS can be injection, compression and transfer molded. Other uses are structural parts as well as circuit breakers.

Information provided by Bulk Molding Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.69 - 1.89 g/ccMolded
Linear Mold Shrinkage 0.0020 - 0.0030 in/in
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 40 - 50
Tensile Strength 9500 - 11500 psi
Flexural Strength 34500 - 38500 psi
Flexural Modulus 2000 - 2300 ksi
Compressive Strength 19000 - 23000 psi
Izod Impact, Notched 14.0 - 16.0 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 335 - 385 V/milshort time
Arc Resistance >= 183 sec
Comparative Tracking Index >= 500 V
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 500 °F
Flammability, UL94 V-0UL 94 V0/UL 94 5V
 
Processing PropertiesOriginal ValueComments
Processing Temperature 280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman BMC 1412 Flame and Track Resistant
A. Schulman BMC T40(25)-XHS-15869 Die Casting Replacement Grade Molding Compound
A. Schulman BMC T40(18)-LS Die Casting Replacement Grade Molding Compound
A. Schulman BMC A50-XHS-U Bulk molding compound
A. Schulman BMC A50-XHS Bulk molding compound

PBMC941 / 123405

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.