MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arla ATECH® 3300 ABS Sheet
Categories: Polymer; Thermoset; Phenolic

Material Notes: ATECH is a series of sheets based on ABS which is a raw material with very high impact-strength. ABS also has impressive thermal qualities and is easy to thermoform and fabricate. The ATECH 3300 is a super high impact ABS with a semigloss top layer of ASA material.
Also Available In: ATECH 3300M with a matte ASA surface; ATECH 3330 with ASA surface on both sides
Recycling: The total recycling concept (TRC) covers all types of sheets to provide cost savings. Off-cuts from the sheets can be used in production of new sheets by co-extruding virgin material as the top layer. Care is taken that all quality requirements are met.

Benefits: Weathering performance; Chemical resistance; Easy to thermoform; High impact strength; Good thermal qualities

Application: The weathering properties makes ATECH 3300 the ultimate choice for any outdoor application such as gardening applications, agriculture vehicles, transport vehicles etc.

Information provided by Arla Plast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Linear Mold Shrinkage 0.0060 - 0.0070 cm/cm0.0060 - 0.0070 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 77.0 MPa11200 psiISO 2039
Tensile Strength, Yield 33.0 MPa4790 psiISO 527
Elongation at Break 53 %53 %ISO 527
Elongation at Yield >= 3.0 %>= 3.0 %ISO 527
Tensile Modulus 1.90 GPa276 ksiISO 527
Flexural Strength 55.0 MPa7980 psiISO 178
Flexural Modulus 2.00 GPa290 ksiISO 178
Izod Impact, Notched (ISO) 30.0 kJ/m²14.3 ft-lb/in²ISO 180
Izod Impact, Unnotched (ISO)  10.0 kJ/m²
@Temperature -35.0 °C
4.76 ft-lb/in²
@Temperature -31.0 °F
ISO 180
 20.0 kJ/m²
@Temperature -18.0 °C
9.52 ft-lb/in²
@Temperature -0.400 °F
ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C187 °FISO 75-2
Vicat Softening Point 97.0 °C207 °FB120; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARLA904 / 301082

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.