MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Controltac™ IJ380Cv3 Wrap Film with Comply™ v3 Adhesive
Categories: Polymer; Film

Material Notes: 2-mil white, vinyl film with a luster finish; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Non-visible, air release channels for fast, easy, bubble-free installations; Superior conformability and lift resistance; perfect for vehicle wraps with deep channels or concave areas-Stretch selected finished graphic constructions up to 150% (ie a 10 in film piece can stretch to 15 inches) without primer or relief cuts and maintain lift resistance; see details and exceptions in Section 10; Removable with heat and/or chemicals

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milwithout adhesive
 76.2 - 102 microns3.00 - 4.00 milwith adhesive
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 13.8 MPa2000 psi
Peel Strength 0.526 - 0.877 kN/m3.00 - 5.00 pliAdhesion to Automotive clear coats
 0.701 - 0.877 kN/m4.00 - 5.00 pliAdhesion to ABS
 0.701 - 0.877 kN/m4.00 - 5.00 pliAdhesion to Acrylic enamel
 1.23 - 1.40 kN/m7.00 - 8.00 pliAdhesion to Aluminum, anodized

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
IRPC Polimaxx Polene BM3245 PC High Density Polyethylene

PMM34823 / 169570

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.