MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unifrax Isofrax® 1260C High Index Fiber Thermal Insulation
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Isofrax® Thermal Insulation from Unifrax is a fiber that utilizes a unique, patented silica-magnesia chemistry to solve a variety of demanding, high-temperature application problems. Isofrax 1260C Fiber is the product of a long-term research and development effort by Unifrax to produce a fiber which has the high-temperature performance characteristics required in many applications at temperatures up to 1260°C/2300°F and also meets European and German regulatory requirements. Isofrax 1260C Fibers provide high-temperature stability, low thermal conductivity, low heat storage, thermal shock resistance, and low weight. Isofrax 1260C Fiber exhibits excellent chemical stability and resistance to attack from most corrosive agents. Exceptions include hydrofluoric acids, phosphoric acid and strong alkalies. Isofrax 1260C Fiber also provides superior wetting resistance to molten aluminum alloys at high temperatures.

Isofrax High Index Fiber is a material which has a reduced amount of shot or unfiberized material. This high index fiber can be a good reinforcement material for automotive brake linings or can be used as a mechanical thixotrope in fire-resistant coatings.

Applications: Isofrax 1260C Fiber is currently used in the manufacture of many high-temperature product forms such as felts, boards, papers, and vacuum cast shapes. This product can also be used as a high-temperature fill or packing material in a variety of applications, such as refractory expansion joints, furnace base seals, tube seals, and for packaging around burner tiles. Additional applications include reinforcement or fillers infriction materials and composites, and thixotropic agents in coatings and adhesives.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.54 g/cc
 
Thermal PropertiesOriginal ValueComments
Melting Point 1500 °C
Maximum Service Temperature, Air 1260 °CRecommended Operating Temperature
 
Component Elements PropertiesOriginal ValueComments
MgO 18 - 27 %
Other, total 0.00 - 4.0 %Trace Elements
SiO2 70 - 80 %
 
Descriptive Properties
ColorBluish White
Fiber Diameter (microns)2.0 to 3.0
Fiber Index (%)70-95+
Temperature Grade (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Enfil™ Engineered Fibers Enfil SF Thermal Ceramic
Morgan Advanced Ceramics Enfil™ Engineered Fibers Enfil SH Thermal Ceramic
Unifrax Isofrax® 1260C Blanket Thermal Insulation
Unifrax Fiberfrax® HSA-HP High Purity High-Index Fiber
Unifrax Fiberfrax® HS95C High Purity High-Index Fiber

CUNIF125 / 97897

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.