MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity.

Applications: Used as, among other things, thermal insulation plates where high strength properties are requires.

Information provided by Elektro-Isola

Key Words: IEC/EN 60893-3-1 UP GM 204, DIN 7735 Hm 2472, NF C26 153 Vm P3, BS 3953 UP-5, NEMA LI 1 GPO 1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc
@Temperature 23.0 °C
0.0578 lb/in³
@Temperature 73.4 °F
24h/23°C/50% RH; ISO 1183-A
Water Absorption 0.20 %0.20 %ISO 62-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 150 MPa
@Thickness >=1.50 mm
21800 psi
@Thickness >=0.0591 in
24h/23°C/50% RH; ISO 527
Flexural Strength  100 MPa
@Thickness >=1.50 mm,
Temperature 130 °C
14500 psi
@Thickness >=0.0591 in,
Temperature 266 °F
1 hour at temperature/50% RH, Normal to laminate plane; ISO 178
 250 MPa
@Thickness >=1.50 mm,
Temperature 23.0 °C
36300 psi
@Thickness >=0.0591 in,
Temperature 73.4 °F
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Flexural Modulus 11.0 GPa
@Thickness >=1.50 mm
1600 ksi
@Thickness >=0.0591 in
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Compressive Strength 350 MPa
@Thickness >=5.00 mm
50800 psi
@Thickness >=0.197 in
24h/23°C/50% RH, , Normal to laminate plane; ISO 604
Shear Strength 35.0 MPa
@Thickness >=5.00 mm
5080 psi
@Thickness >=0.197 in
Parallel, 24h/23°C/50% RH; IEC 60893-2
Izod Impact, Notched (ISO) 60.0 kJ/m²
@Thickness >=5.00 mm
28.6 ft-lb/in²
@Thickness >=0.197 in
Parallel, 24h/23°C/50% RH; ISO 180/2A
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 100000 ohm100000 ohmafter immersion in water for 24 hr at 23°C; IEC 60167
Dielectric Constant  4.0
@Thickness <=3.00 mm,
Frequency 50 Hz
4.0
@Thickness <=0.118 in,
Frequency 50 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
 4.0
@Thickness <=3.00 mm,
Frequency 1e+6 Hz
4.0
@Thickness <=0.118 in,
Frequency 1e+6 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
Dielectric Strength  2.36 kV/mm
@Thickness >=3.00 mm,
Temperature 90.0 °C
60.0 kV/in
@Thickness >=0.118 in,
Temperature 194 °F
after 1 hour in oil, Parallel to laminate plane; IEC 60243-1
 10.0 kV/mm
@Thickness 3.00 mm,
Temperature 90.0 °C
254 kV/in
@Thickness 0.118 in,
Temperature 194 °F
after 1 hour in oil, Normal to laminate plane; IEC 60243-1
Dissipation Factor  0.010
@Thickness <=3.00 mm,
Frequency 50 Hz
0.010
@Thickness <=0.118 in,
Frequency 50 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
 0.010
@Thickness <=3.00 mm,
Frequency 1e+6 Hz
0.010
@Thickness <=0.118 in,
Frequency 1e+6 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
Comparative Tracking Index 600 V
@Thickness >=3.00 mm
600 V
@Thickness >=0.118 in
24h/23°C/50% RH; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 °C
@Thickness >=3.00 mm,
Time 7.20e+7 sec
356 °F
@Thickness >=0.118 in,
Time 20000 hour
IEC 60216
 
Descriptive Properties
ColorCream

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PELEKT055 / 126931

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.