MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik EUROPLEX® SDX Polycarbonate Sheet  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: EUROPLEX® SDX Glazings dissipate electric charges in a controlled way against earth. EUROPLEX® SDX for planar installations.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPaISO 527
Tensile Strength, Yield 60.0 MPaISO 527
Elongation at Break 6.0 %Edge fiber at bending strength; ISO 178
 70 %ISO 527
Modulus of Elasticity 2.40 GPaISO 527
Flexural Strength 80.0 MPaat 3.5%; ISO 178
 100 MPaISO 178
Flexural Modulus 2.10 GPaISO 178
Compressive Yield Strength 70.0 MPaISO 604
Compressive Strength 70.0 MPaISO 604
Compressive Modulus 2400 MPaISO 604
Charpy Impact Unnotched NBISO 179
Charpy Impact, Notched 11.0 kJ/m²ISO 179
Abrasion 2.5Taber; ASTM D1004
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1e+05 - 1.00e+7 ohmDIN IEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µin/in-°FASTM D969
Vicat Softening Point 145 °CISO 306
 
Optical PropertiesOriginal ValueComments
Haze 1.2 %ASTM D1003
Transmission, Visible 80 %DIN 5030, DIN 5036
 
Descriptive Properties
Extensibility0.06ISO 527
Nominal compression at compression strength0.08ISO 604

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NUDEC® PC Polycarbonate Sheet
Evonik Cyrolon® AR Polycarbonate Sheet
Overview of materials for Nylon 63, 35% Glass-Filled
3M FL012 Lexan Label Product
Trinseo Plexiglas® V052 Acrylic

PEVONIL189 / 196393

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.