MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

1370 Aluminum
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 1000 Series Aluminum

Material Notes: Used for electrical applications. Very good weldability. Property data provided by PCP-Canada for heat treated cast and sawn ingots.

Composition Notes:
The aluminum content for unalloyed aluminum not made by a refining process is the difference between 100.00 percent and the sum of all other analyzed metallic elements present in amounts of 0.010 percent of more each, expressed to the second decimal before determining the sum. For alloys and unalloyed aluminum not made by a refining process, when the specified maximum limit is 0.XX, an observed value or a calculated value greater than 0.005 but less than 0.010% is rounded off and shown as " less than 0.01%".
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A91370; Aluminium 1370; AA1370; Al1370
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.70 g/cc0.0975 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 83.0 MPa12000 psi
Tensile Strength, Yield 28.0 MPa4060 psi
Elongation at Break 28 %28 %
Modulus of Elasticity 68.9 GPa9990 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000280 ohm-cm0.00000280 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.8 µm/m-°C
@Temperature 20.0 - 100 °C
13.2 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 234 W/m-K1620 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al >= 99.70 %>= 99.70 %Specified
Boron, B <= 0.02 %<= 0.02 %
Chromium, Cr <= 0.01 %<= 0.01 %
Copper, Cu <= 0.02 %<= 0.02 %
Gallium, Ga <= 0.03 %<= 0.03 %
Iron, Fe <= 0.25 %<= 0.25 %
Magnesium, Mg <= 0.02 %<= 0.02 %
Manganese, Mn <= 0.01 %<= 0.01 %
Other, each <= 0.02 %<= 0.02 %
Other, total <= 0.10 %<= 0.10 %
Silicon, Si <= 0.10 %<= 0.10 %
V+Ti >= 0.02 %>= 0.02 %
Zinc, Zn <= 0.04 %<= 0.04 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 1350-O
Aluminum 1100-O
Aluminum 1060-O
Aluminum 1050-H14
Aluminum 1350-H19

MA1370 / 8811

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.