OKULEN® 2000 - Certec – FN1450 is a special UHMW-PE Polymer-compound (9 mio. g/mol). With this special fillers we reach a very high up to extremely high wear resistance and excellent sliding properties. Properties: Extremely wear resistant; Good sliding properties; Good chemical resistance Color: pearl white FN1450/similar RAL1013 Range of applications: Paper industry (High-Tech-Paper-Machines) Information provided by Okulen |