MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Durez® 152 Phenolic, Compression Grade
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Mineral/Fiber Filled

Material Notes: Durez 152 Phenolic is a two-stage, heat resistant/electrical molding material. It exhibits superior dimensional stability, good strength retention at elevated temperature and good molded appearance and machinability which account for its widespread use on electrical, telecommunication and appliance applications.

Durez 152 is fungus resistant per Mil-I-631D and Mil-E-5272C

Information provided by Sumitomo Bakelite North America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.5 g/ccASTM D792
Apparent Bulk Density 0.68 g/ccASTM D1895
Water Absorption 0.3 %ASTM D570
Linear Mold Shrinkage 0.010 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 48 MPaASTM D638
Tensile Modulus 9.6 GPaASTM D638
Flexural Strength 76 MPa
Compressive Strength 207 MPaASTM D695
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+12 ohm-cmASTM D257
Dielectric Constant 5.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 12.8 kV/mmStep by step; ASTM D149
 14.7 kV/mmShort Time; ASTM D149
Dissipation Factor 0.050
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 190 VIEC Tracking Index
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 160 °CUL temperature Index
Deflection Temperature at 1.8 MPa (264 psi) 191 °CASTM D648
Flammability, UL94 V-1
@Thickness 1.50 mm
 V-0
@Thickness 3.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade
Sumitomo Bakelite Durez® 118 Phenolic, Compression Grade
Sumitomo Bakelite Durez® 153 Phenolic, Compression Grade
Plywood
Sumitomo Bakelite Durez® 156 Phenolic, Compression Grade

P90X09a / 142664

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.