MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ SI Gel Surface Insensitive Instant Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: 3M™ Scotch-Weld™ Surface Insensitive Adhesives bond rough, porous, contaminated, and acidic substrates including wood, cardboard, veneer, fabric, cork, and leather. SI Gel (formerly SB09) is a fast curing, very high viscosity, gap filling cyanoacrylate. Its gel formation can be used for bonding poorly mating components and for porous substrates such as china and other ceramics and can be used on vertical surface as it will not drip or slump.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccUncured
Brookfield Viscosity 7000 - 20000 cPRVT 'T-spindle' C @ 20 rpm
 50000 - 90000 cPRVT 'T-spindle' C @ 2.5 rpm
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 2900 psicured; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 82.0 °C
Minimum Service Temperature, Air -54.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 - 1.00 minTime to Handling Strength
 24.0 hourFull Cure
 
Descriptive Properties
AppearanceClear Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM34707 / 169454

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.