MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Poco Graphite AXF-5F Biomedical Grade Graphite  (discontinued **)
Categories: Carbon; Graphite

Material Notes: POCO has developed post synthesis modifications to make our graphites more suitable to specific conditions. As a producer of highly technical, specialty materials, POCO also offers design engineering support, precision machining, and material testing. Diverse applications include precision parts, graphite filters for blood dialysis machines, graphite electrodes and heating elements.
The compatibility of carbon and graphite with human tissues and bodily fluids have allowed POCO materials to be used in a variety of implants. Applications include artificial heart valves, dental mounts, cancer treatment devices and blood analysis devices.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Apparent Bulk Density 1.78 g/cc0.0643 lb/in³
Particle Size 5.0 µm5.0 µm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7474
Flexural Strength 90.0 MPa13100 psi
Compressive Strength 145 MPa21000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00147 ohm-cm0.00147 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 95.0 W/m-K659 BTU-in/hr-ft²-°F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Graphite, Carbon, C
BACT Metal-Dylyn® Diamond-Like Nanocomposite Coating
BACT Dylyn® Diamond-Like Nanocomposite Coating
BACT DLC Diamond-Like Coating
Aremco Pyro-Paint™ 634-GR High Temperature Refractory Coating, GR >95%

CPOCO26 / 85603

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.