MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Acerde Silicon Carbide
Categories: Ceramic; Carbide

Material Notes: Silicon Carbide key properties: High oxidation resistance, High hardness, Resistive to thermal stress, High thermal conductivity, Low thermal expansion, High elastic modulus, Superior chemical inertness

Silicon Carbide main applications domains: Refractories (furnace protection, nuclear, aerospace), Heating apparatus (Resistivity heaters, holders), Machining tools (cutting tools, abrasive, friction), Chemistry (catalyst holders, medical), Optics (mirrors for telescope), Crucibles (foundries), Susceptors

Information provided by Acerde

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.21 g/cc
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 2800
Tensile Modulus 420 GPa
Flexural Strength 610 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 100 - 1.00e+6 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.00 - 5.00 µm/m-°C
@Temperature <=1000 °C
Thermal Conductivity 63.0 - 155 W/m-K
@Temperature 20.0 °C
Melting Point 2730 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Carbide, Alpha SiC
Silicon, Si
CeramTec Rocar® ST Silicon Carbide, SSiC
Silicon Carbide, sublimed
CeramTec Rocar® S Silicon Carbide, SSiC

CZACERD01 / 122019

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.