MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sipchem Sahara C 1000HT Polypropylene, Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Description: SAHARA C 1000HT is a nucleated impact copolymer with antistatic additives used for injection molding applications. It exhibits an outstanding balance of mechanical properties combined with a high fluidity. Sahara C 1000 HT is used in housewares and in thin-walled containers for food packaging (e.g. margarine tubs, yoghurt pots, etc.) and compounding applications. This grade is not intended for medical and pharmaceutical applications.

Product Characteristics:
Commercial Status: Experimental grade.
Processing Method: Injection Molding
Typical applications: Thin wall containers; housewares.

Information provided by Sahara International Petrochemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO1183-1
Melt Flow 100 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 27.0 MPaISO 527-1, -2
Elongation at Break 3.6 %ISO 527-1, -2
Elongation at Yield 3.1 %ISO 527-1, -2
Tensile Modulus 1690 MPaISO 527-1, -2
Flexural Modulus 1690 MPaISO 178
Izod Impact, Notched 2.80 J/mISO 180
Charpy Impact, Notched 2.00 kJ/m²
@Temperature -20.0 °C
Type 1, Edgewise; ISO 179
 2.10 kJ/m²
@Temperature 0.000 °C
Type 1, Edgewise; ISO 179
 3.50 kJ/m²
@Temperature 23.0 °C
Type 1, Edgewise; ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 108 °Cunannealed; ISO 75B-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °Cunannealed; ISO 75B-1, -2
Vicat Softening Point 73.0 °CB50; ISO 306
 147 °CA50; ISO 306
Shrinkage 1.0 - 2.5 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature 210 - 250 °CBarrel temperature range
Melt Temperature 240 - 260 °C
Mold Temperature 15.0 - 40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIPCH038 / 285351

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.