MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Röchling Lignostone® Transformerwood® LI/2-E3 Laminated densified wood
Categories: Polymer; Thermoset; Wood and Natural Products; Wood

Material Notes: Lignostone® Transformerwood® is a laminated densified wood according to IEC 61061. It consists of red beech veneers, which are joined together with thermosetting synthetic resins under high pressure and heat. Lignostone® Transformerwood® has the following properties:
  • Good electrical insulation properties
  • High mechanical strength at low specific density
  • Easy and fast to dry
  • Very good oil absorption

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.850 g/ccIEC 61061
Oil Absorption 30 %IEC 601061
Moisture Absorption 5.00 %IEC 601061
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 11.0 GPaPerpendicular, 500x20x20 mm, Support distance: 320 mm; DIN EN ISO 178
Flexural Strength 140 MPaPerpendicular, 500x20x20 mm, Support distance: 320 mm; DIN EN ISO 178
Compressive Strength 55.0 MPaParallel, 10x10x10 mm; DIN EN ISO 604
 100 MPaPerpendicular, 10x10x10 mm; DIN EN ISO 604
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 60093
Dielectric Constant 3.7100x100x10 mm, oil impregnated; IEC 60250
Dielectric Strength 15.0 kV/mm
@Thickness 76.2 mm,
Temperature 90.0 °C
[kV/ 3mm], perpendicular, SQ; IEC 600243
 16.7 kV/mm
@Thickness 76.2 mm,
Temperature 90.0 °C
[kV/ 3mm], perpendicular, HQ; IEC 600243
 18.3 kV/mm
@Thickness 76.2 mm,
Temperature 90.0 °C
[kV/ 3mm], perpendicular, TQ; IEC 600243
 70.0 kV/in
@Thickness 25.0 mm,
Temperature 90.0 °C
Perpendicular, SQ; IEC 600243
 80.0 kV/in
@Thickness 25.0 mm,
Temperature 90.0 °C
Perpendicular, HQ; IEC 600243
 90.0 kV/in
@Thickness 25.0 mm,
Temperature 90.0 °C
Perpendicular, TQ; IEC 600243
Dissipation Factor 0.010
@Frequency 50 Hz
100x100x10 mm, oil impregnated; IEC 60250
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 221 °FDIN 7707

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ferrite 5, Sintered Iron-Strontium Oxide Hard Magnetic Material
96% Alumina, thick-film, as fired
Ferrite A, Bonded Iron-Barium Oxide Hard Magnetic Material
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
Celanese Ateva® 2820A Ethylene Vinyl Acetate Copolymer

PROCH9112 / 232815

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.