MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Parker Chomerics CHO-THERM® 1678 High Power Thermally Conductive Electrical Insulator Pad
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: CHO-THERM® high-power thermal insulator pads are thermally conductive materials designed for use where the highest possible thermal, dielectric, and mechanical properties are required. Fiberglass cloth reinforcement strengthens CHO-THERM® pads against tear, cut-through and punctures. These materials are available in sheet form and die-cut configurations. An optional acrylic adhesive layer (with PSA) is available on one or two sides. With a proven track record spanning several decades in multiple applications, these products are the first choice for high-end power supplies, industrial, aerospace, and military/avionics applications.

Features/Benefits: Excellent thermal properties, High dielectric strength, Excellent mechanical strength and puncture resistance, 100% inspected for dielectric properties on every sheet, PSA attachment option available, Meets RoHS specifications, and Proven through decades of use in demanding military and aerospace applications.

Typical Applications: Power conversion equipment, Power supplies and UPS, Power semiconductors, Automotive electronics, Motor and engine controllers, and Televisions and consumer electronics

Product Attributes: Highest reliability in rigorous applications and Proven in aerospace/defense applications.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.55 g/ccASTM D792
Thickness 200 - 300 micronsASTM D374
Outgassing - Total Mass Loss 0.55 %TML; ASTM E595
Collected Volatile Condensable Material 0.12 %ASTM E595
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Tensile Strength 3000 psiASTM D412
Elongation at Break 20 %ASTM D412
Tear Strength 200 pliASTM D642
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.6
@Frequency 1e+6 Hz
ASTM D150
Dielectric Breakdown 2500 VASTM D149
Dissipation Factor 0.0070
@Frequency 1e+6 Hz
Chomerics Test
 
Thermal PropertiesOriginal ValueComments
CTE, linear 250 µm/m-°CASTM E831
Specific Heat Capacity 1.00 J/g-°CASTM E1296
Thermal Conductivity 2.00 W/m-KASTM D5470
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -40.0 °C
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 MonthMonths for shipment, with PSA; Chomerics
 24.0 MonthMonths for shipment, Dry Pad; Chomerics
 
Descriptive Properties
CarrierFiberglass
ColorPink

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elantas Conap RN-1000 / EA-02 Conapoxy® Resin / Conacure® Hardener
ChevronTexaco URSA® SAE 50 Super Plus

PCHOME251 / 130961

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.