MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SIMONA America SIMONA® 010024311 ECTFE 901 Welding Rods
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: Offers exceptional chemical resistance up to 300°F (149°C). FM 4910 compliant for semiconductor clean room applications. This material features high purity, and is suitable for wetted parts.

Information provided by Simona America Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.68 g/ccASTM D792
Water Absorption <= 0.010 %ASTM D570
Thickness 125 mil
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 73ASTM D2240
Tensile Strength, Yield 4500 psiASTM D638
Elongation at Break 255 %ASTM D638
Flexural Modulus 245000 psiASTM D638
Izod Impact, Notched NBASTM D256
Coefficient of Friction, Dynamic 0.20ASTM C1894
Coefficient of Friction, Static 0.10ASTM C1894
Taber Abrasion, mg/1000 Cycles 5.0Taber CS 17
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µin/in-°FASTM D696
Melting Point 468 °FASTM D3418
Maximum Service Temperature, Air 302 °F
Deflection Temperature at 0.46 MPa (66 psi) 195 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 160 °FASTM D648
Flammability, UL94 V-0
 
Descriptive Properties
Colornatural
Regulatory CodeFM 4910

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIMONA579 / 285307

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.