MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Saint-Gobain Versilon™ SE-200 Inert Tubing Formulation
Categories: Polymer; Thermoplastic

Material Notes: Formerly Tygon® SE-200. Without sacrificing the flexibility, glass-like clarity or outstanding bend radius for which Tygon® tubing is known, Tygon® Inert Tubing can handle many applications where flexible tubing of the past could not be used. Its FEP inner liner provides the ultimate in chemical resistance and can handle a wide variety of fluids from corrosives to MEK-based solvents. The liner is inert, meaning it will not extract or contaminate fluids being transferred. The fluid path will not impart odor or taste, making it well-suited for food and beverage use. It meets FDA criteria for food and beverage applications, as well as USP Class VI criteria for biocompatibility. Tygon® Inert Tubing combines all the benefits of Tygon® with the inertness of a fluoropolymer, providing superior performance in many applications and industries.

Features/Benefits:
  • Crystal Clarity
  • Improved flexibility when compared to rigid fluoropolymer tubings
  • Chemically resistant and inert
  • Non-contaminating fluid path
  • Meets FDA and USP Class VI Criteria
Typical applications include Chemical Processing, Pharmaceutical Processing and Filling, Paint and Solvent Production and Packaging, Adhesive Transfer Lines, Semiconductor Processing, Photographic Processing Equipment, Beverage Dispensing, Ink and Toner Feed Lines, Fertilizer and Pesticide Distribution.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792-91
Water Absorption <= 0.010 %24 hours at 23°C; ASTM D570-95
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 6615 seconds; ASTM D2240-97
Tensile Strength, Yield 2200 psiASTM D412-97
Elongation at Break 390 %ASTM D412-97
200% Modulus 1379 psi
@Strain 200 %
Tear Strength 250 pliInitial Tear Strength; ASTM D1004-93
Compression Set 59 %
@Temperature 70.0 °C
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
Tensile Set 57 %ASTM D412-97
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 165 °F
Brittleness Temperature -32.0 °FASTM D746-95
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSTGQZ189 / 68703

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.