General Description: PB900, homopolymer made by micro-suspension seeded polymerization, is PVC resin with pseudo plastic flow property. PB900 can be used for wall paper made by knife coating/rotary screen coating. Main Applications: Wall coverings CAS No: 9002-86-2 Information provided by LG Chemical |