MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Total XSene® XRC 20 B High Density Polyethylene - Pipes and Fittings
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: This product is a Total Ecosolutions grade.

HDPE XRC 20 B is a very high performance hexene-based black compound, with a MRS 10 MPa - PE100 classification, particularly appropriate for pressure pipes that are either installed or operated under extreme conditions.

Key characteristics are

  • an extremely high resistance to crack initiation and to slow crack growth
  • meeting the highest prescription and standards for PE pipe
  • Easy processing and safe welding properties.

Designation ISO 1872-PE,E/M-ACGHL,50-T003

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.958 g/cc0.958 g/ccISO 1183
Carbon Black Loading 2.0 - 2.5 %2.0 - 2.5 %ISO 6964
Melt Flow 0.30 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.30 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133/T
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 220 °C374 - 428 °FExtrusion
 200 - 260 °C392 - 500 °FInjection
 
Descriptive Properties
Carbon Black Dispersion, Rating= 3ISO 18553
Thermal Stability 200°C> 20 minEN 728 / ISO 11357-6
Water Content= 300 ppmEN 12118, measured at the stage of compound manufacturing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total XLS 12 B High Density Polyethylene - Pipes and Fittings
Total XT25N High Density Polyethylene, Pipe Resin
Borealis Borstar® HE3492-LS Yellow-Orange High Density Polyethylene for Natural Gas Pipes
Borealis BorSafe™ HE3490-LS Black High Density Polyethylene for Pressure Pipes
Total 53090 High Density Polyethylene - Blow Molding

PTOTAL728 / 130453

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.