System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
BASF Ultramid® A3Z HP UV PA66 (Dry)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Impact Grade
Material Notes:
Ultramid A3Z HP UV is an impact modified PA66 containing heat and ultraviolet light stabilizers. Designed for maximum toughness at low temperatures, Ultramid A3Z HP UV offers a unique combination of impact performance and excellent processability.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.08
g/cc
ISO 1183
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
46.0
MPa
50mm/min; ISO 527
Elongation at Break
50 %
50mm/min, Nominal strain; ISO 527
Flexural Modulus
1703
MPa
ISO Data
Izod Impact, Notched (ISO)
83.0
kJ/m²
ISO Test
22.0
kJ/m²
@Temperature -40.0 °C
ISO Test
Thermal Properties
Original Value
Comments
Melting Point
258
°C
10 K/min
258
°C
ASTM Test
Deflection Temperature at 1.8 MPa (264 psi)
63.0
°C
ISO 75
Descriptive Properties
Color
Natural
Commercial Status
Active America
Impact Modified
Yes
Primary Processing Technique
Injection Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
BASF Ultramid® A3Z HP PA66 (Dry)
BASF Ultramid® A3Z HP BK20465 PA66 (Dry)
Envalior Akulon® K222-DL PA6, Dry, Low Viscosity, Heat Stabilized, Light Stabilized
BASF Ultramid® A3Z HP UV BK23220 PA66 (Dry)
BASF Ultramid® A3L HP UV BK 23220 PA66 (Dry)
PBASF9279 / 85043
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.