MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Proto3000 17-4 PH MIM - MPIF 35 Stainless Steel, As-Sintered
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Ferrous Metal; Stainless Steel; Precipitation Hardening Stainless

Material Notes: This metal alloy is the perfect choice for the traditional operating environments of a manufacturing floor. It can be heat-treated to a variety of hardness and toughness levels, allowing users to customize the post-sintering properties in order to suit a wide variety of applications.

Applications

  • Manufacturing Machinery
  • Pump Components
  • Chemical Processing
  • Valving, Fasteners
  • Food Processing
  • Jigs and Fixtures

Property data per MPIF Standard 35.

Information provided by Proto3000

Key Words: UNS S17400, EN 1.4542, ISO 4542-174-00-I
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.50 g/ccASTM B311
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 27.0ASTM E18
Tensile Strength, Ultimate 790 MPaASTM E8M
Tensile Stress 200 MPa
@Strain 0.1 %
 800 MPa
@Strain 0.9 %
 950 MPa
@Strain 1.5 %
Tensile Strength, Yield 650 MPaASTM E8M
Elongation at Break 4.00 %ASTM E8M
Modulus of Elasticity 190 GPaASTM E8M
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.0700 %
Chromium, Cr 15.5 - 17.5 %
Copper, Cu 3.00 - 5.00 %
Iron, Fe 69.98 - 78.35 %Balance
Manganese, Mn <= 1.00 %
Nb + Ta 0.150 - 0.450 %
Nickel, Ni 3.00 - 5.00 %
Silicon, Si <= 1.00 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NPROTO876 / 322889

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.