MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 6069-T6, 1.25 Round Bar, Hot Hollow Extrusion, Average Tensile Values
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 6000 Series Aluminum Alloy

Material Notes: Heat treatable Mg-Si-Cu aluminum alloy. Tests indicate a tensile ultimate and yield strength in the T6 condition about 40% higher than its sister 6061 alloy and essentially equal to the tensile properties of 6013-T6 sheet. Corrosion resistance does not appear to be inferior to 6061. Present applications are high pressure seamless gas containers formed by either hot or cold impact extrusion and tubing for light weight bicycle frames.

Information provided by Northwest Aluminum Company.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 6069-T6; UNS A96069; Al6069-T6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.72 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 442 MPaTransverse
 478 MPaLongitudinal
Tensile Strength, Yield 397 MPaTransverse
 447 MPaLongitudinal
Elongation at Break 13 %Transverse
 14.4 %Longitudinal
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000450 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 23.6 µm/m-°C
@Temperature 20.0 - 100 °C
Melting Point 581 - 648 °C
Solidus 581 °C
Liquidus 648 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 94.8 - 97.5 %As remainder
Chromium, Cr 0.05 - 0.30 %
Copper, Cu 0.55 - 1.0 %
Iron, Fe <= 0.40 %
Magnesium, Mg 1.2 - 1.6 %
Manganese, Mn <= 0.05 %
Other, each <= 0.05 %
Other, total <= 0.15 %
Silicon, Si 0.60 - 1.2 %
Strontium, Sr <= 0.05 %
Titanium, Ti <= 0.10 %
Vanadium, V 0.10 - 0.30 %
Zinc, Zn <= 0.05 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 6069-T6, 0.5 in x 3 in. Bar, Hot Hollow Extrusion, Average Tensile Values
Aluminum 6069-T6, 0.75 in x 2.2 in. Bar, Hot Hollow Extrusion, Average Tensile Values
Aluminum 6069-T6, Hot Hollow Extrusion, Average Tensile Values
Aluminum 6061-T6; 6061-T651
Aluminum 6069-T6, Cold Impact Extruded Cylinder, Minimum Tensile Values

MA6069T6C / 9414

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.