MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Magnesium
Magnesium Elektron - Service & Innovation in Magnesium

(Viewing data as-entered. Click here to return)
Magnesium Elektron Elektron® 675 Magnesium Wrought Alloy
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: High strength wrought Mg alloy used for high performance components, including at elevated temperature. Excellent corrosion resistance and easily machined. Can be extruded, forged and hot formed. Supplied in the T5 condition.

Key Words: AMS 2154 Class AA
Vendors: Magnesium Elektron is the world leader in high strength magnesium alloys in rolled, extruded and cast forms. Phone (303) 589-3189 or visit www.magnesium-elektron.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.95 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 110 - 118
Tensile Strength 32.0 ksi
@Temperature 300 °C
 57.0 ksi
@Temperature 200 °C
 58.0 ksi
@Temperature 100 °C
 59.0 ksi
@Temperature 20.0 °C
Tensile Strength, Yield 18.0 ksi
@Strain 0.2 %,
Temperature 300 °C
 43.5 ksi
@Strain 0.2 %,
Temperature 100 °C
 43.5 ksi
@Strain 0.2 %,
Temperature 200 °C
 45.0 ksi
@Strain 0.2 %,
Temperature 20.0 °C
Elongation at Break 9.0 %
Fatigue Strength 29000 psi
@# of Cycles 5.00e+7
Axial; R = 0.1; Extruded Bar; ASTM E466
Fracture Toughness 14.6 ksi-in½KQ
 
Thermal PropertiesOriginal ValueComments
CTE, linear 27.4 µm/m-°C
Thermal Conductivity 76.0 W/m-K
 
Descriptive Properties
Corrosion Resistance10 - 40 MpyASTM B117 salt spray
Stress Corrosion CrackingPasses ASTM G44

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium Elektron Elektron® ZK60A Magnesium Alloy, UNS M16600
Magnesium EA55RS-T4, Extruded
Magnesium EA65RS-T4, Extruded
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy
SAE SiC/AZ91 Magnesium Matrix Composite, as cast

NMAGEL900 / 147649

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.