MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom PLASTALEN® PQ 83 T 30 Polypropylene reinforced with mineral filler  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Impact modified PP for injection molding with the content of 30 % mineral filler. Application in automotive industry. Delivered in black grade.

Information Provided by Plastcom spol. s r.o.

Key Words: STN EN ISO 1043-1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³STN EN ISO 1183-1
Filler Content 30 %30 %
Linear Mold Shrinkage 0.013 cm/cm0.013 in/inSTN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.015 cm/cm0.015 in/inSTN EN ISO 294-4
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 13.0 MPa1890 psiSTN EN ISO 527-2
Elongation at Break 3.0 %3.0 %STN EN ISO 527-2
Tensile Modulus 1.50 GPa218 ksiSTN EN ISO 527-2
Flexural Strength 20.0 MPa2900 psiSTN EN ISO 178
Flexural Modulus 1.25 GPa181 ksiSTN EN ISO 178
Charpy Impact Unnotched  2.20 J/cm²
@Temperature -20.0 °C
10.5 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched  0.350 J/cm²
@Temperature -20.0 °C
1.67 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 °C320 °FSTN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C162 °FSTN EN ISO 75-2 (A)
Vicat Softening Point 117 °C243 °FSTN EN ISO 306
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 250 °C392 - 482 °F
Mold Temperature 40.0 - 70.0 °C104 - 158 °F
Drying Temperature 80.0 °C
@Time 14400 sec
176 °F
@Time 4.00 hour
Moisture Content 0.10 %0.10 %STN EN ISO 3344
Injection Pressure 70.0 - 120 MPa10200 - 17400 psi
 
Descriptive Properties
ColorBlack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostacom DKC 179N C12334 Polypropylene, Mineral Reinforced
LG Chemical LUPOL HG-3200 High Gloss Polypropylene, 20% Mineral Fillers
ExxonMobil PP1404FC Mineral-filled Homopolymer
Eurotec® Tecolen® CP20 MF20 NL XA70 PPCP, 20% mineral filled, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Cossa Polimeri ESTAPROP H 10100 BS Polypropylene, 50% Mineral Filled

PPLACO605 / 140876

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.