MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics AL 300 ™ Mac-A976W Aluminum Oxide Ceramic
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: A top quality alumina ceramic of 97.6% Al2O3 content, widely used for high integrity components where its exceptional electrical and thermal properties are essential to operational stability and reliability.

Prime Features:

  • Exceptionally high dielectric strength
  • Consistent dielectric constant
  • Dense, non-porous and vacuum tight
  • Readily accepts moly-manganese metallizing for high temperature brazing of assemblies
  • Electrically and dimensionally stable across a wide temperature range
  • Resists chemical attack and abrasion
  • Good thermal conductivity
Typical Applications:
  • High power tubes for klystron and x-ray equipment used in defence, medical and communications
  • Electro-optical equipment
  • Flow measurement devices
  • Pressure sensors
  • Power distribution equipment
Production Capabilities:
  • Isostatic and dry pressing of small to large complex components
  • CNC grinding and lapping to very tight tolerances
  • Prototype, batch and volume production
  • Complete documentation and traceability
  • Functional coating, such as Cr2O3, MnTiCr.0.

Information provided by Morgan Advanced Materials

Key Words: Mac-A976W
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.76 g/ccfired
Open Porosity 0.00 %fully dense, % nominal, apparent
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell HR45N 75
Flexural Strength 296 MPa
Compressive Strength >= 1720 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 8.40e+10 ohm-cm
@Temperature 500 °C
 1.00e+12 ohm-cm
@Temperature 300 °C
 >= 1.00e+14 ohm-cm
@Temperature 25.0 °C
Dielectric Constant 9.0
@Frequency 1e+8 Hz,
Temperature 25.0 °C
 9.04
@Frequency 8.50e+9 Hz,
Temperature 25.0 °C
 9.32
@Frequency 8.50e+9 Hz,
Temperature 300 °C
 9.53
@Frequency 1e+7 Hz,
Temperature 25.0 °C
 9.54
@Frequency 8.50e+9 Hz,
Temperature 500 °C
 9.91
@Frequency 1e+7 Hz,
Temperature 300 °C
 10.14
@Frequency 1e+7 Hz,
Temperature 500 °C
Dielectric Strength 43.3 kV/mm
Dissipation Factor 0.000040
@Frequency 1e+7 Hz,
Temperature 25.0 °C
 0.00016
@Frequency 1e+7 Hz,
Temperature 300 °C
 0.00030
@Frequency 1e+8 Hz,
Temperature 25.0 °C
 0.00040
@Frequency 8.50e+9 Hz,
Temperature 300 °C
 0.00045
@Frequency 8.50e+9 Hz,
Temperature 25.0 °C
 0.00052
@Frequency 1e+7 Hz,
Temperature 500 °C
 0.00072
@Frequency 8.50e+9 Hz,
Temperature 500 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.90 µm/m-°C
@Temperature 25.0 - 200 °C
 7.80 µm/m-°C
@Temperature 200 - 400 °C
 8.50 µm/m-°C
@Temperature 400 - 600 °C
 8.80 µm/m-°C
@Temperature 600 - 800 °C
 9.00 µm/m-°C
@Temperature 800 - 1000 °C
Thermal Conductivity 26.8 W/m-K
Maximum Service Temperature, Air 1650 °Cno load
 
Component Elements PropertiesOriginal ValueComments
Al2O3 <= 97.6 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Astro Met AmAlOx 87 Alumina - Aluminum Oxide
CeramTec ATZ Alumina Toughened Zirconia, Dental Grade
Morgan Advanced Ceramics AL-300™ 97-99% Alumina
CeramTec Rubalit® 708 HP Alumina, 96% (High Performance)
CeramTec Ceramtape GC Glass Ceramic

CMORF5004 / 200242

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.