MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Nippon A&L SR-151 SBR
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Type: Non Carboxylated

Special features: Small particle size

Information provided by Nippon A&L

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 50 %50 %
Water Absorption  5.1 %
@Time 10800 sec
5.1 %
@Time 3.00 hour
 15 %
@Time 86400 sec
15 %
@Time 24.0 hour
Particle Size 0.10 µm0.10 µm
pH 7.07.0
Viscosity 250 cP250 cP
Surface Tension 49 dynes/cm49 dynes/cm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 24.6 MPa3570 psi
Elongation at Break 440 %440 %
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -27.0 °C-16.6 °F
 
Descriptive Properties
Gel Content (%)95

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNIPP068 / 267565

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.