3M™ Dyneon™ Fluoroplastic Powder PFA 6503PBZ is a fluorothermoplastic powder with excellent thermal stability characteristics, designed for use in thin film powder coatings. Typical applications include non-stick surfaces, chemical vessel and tank liners, electrical insulation and low friction applications.Information provided by the Dyneon division of 3M. |