MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilon® TSGZ-15 PA666-GF15
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 20% Glass Fiber Reinforced

Material Notes: Product description: Grilon TSGZ-15 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 15% glass fibers. Grilon TSGZ-15 has the following important properties:
  • Good impact strength after molding
  • Good flow behavior
  • Easy processing
Application examples are fictional parts for automotive and mechanical engineering applications such as levers and strips.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccDry; ISO 1183
Water Absorption 8.0 %Sim. to ISO 62
Moisture Absorption 3.00 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 75.0 MPaConditioned; ISO 2039-1
 160 MPaDry; ISO 2039-1
Tensile Strength at Break 65.0 MPaConditioned; ISO 527-1/-2
 110 MPaDry; ISO 527-1/-2
Elongation at Break 4.0 %Dry; ISO 527-1/-2
 10 %Conditioned; ISO 527-1/-2
Tensile Modulus 2900 MPaConditioned; ISO 527-1/-2
 5600 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 70.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 75.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
 90.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 5.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 5.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 17.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+9 ohm-cmConditioned; IEC 60093
 1.00e+11 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+10 ohmIEC 60093
Dielectric Strength 27.0 kV/mmConditioned; IEC 60243-1
 30.0 kV/mmDry; IEC 60243-1
Comparative Tracking Index 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°CISO 11359-1/-2
Melting Point 260 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °CLong Term; ISO 2578
 220 °CShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 215 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 60.0 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveInterior
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
FormGranules
Industry & Consumer goodsHousewares
 Mechanical Engineering
 Power transmission
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Special CharacteristicsHigh impact or impact modified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilon® TSG-15/4 PA666-GF15
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Conditioned)
Ashley Polymers Ashlene® 527LD-14G Nylon 66, 14% Glass Reinforced
Ashley Polymers Ashlene® 527LD-13G Nylon 66, 13% Glass Reinforced
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry)

PGRH290 / 156999

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.