Hostacom CR 250 F is a 15% talc filled elastomeric modified PP, with medium melt flow rate, excellent impact/stiffness balance and very good processability. This grade is delivered in customer customized colors, some properties may be slightly altered upon color selected. Applications: Automotive Parts, Instrument Panels, Interior Automotive Applications.Information provided by LyondellBasell. |