MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Sarlink® TPV X5735B Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 5700B Series are highly engineered extrusion-grade thermoplastic vulcanizates with outstanding UV stability designed for demanding automotive interior and exterior sealing applications, including glass run channels, waistbelts, weather strips, seals and other profiles. This product is a low hardness, low density, high performance grade with low fogging and excellent color retention and elastic properties.

Availability: Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Processability; Low Density; Low Specific Gravity; Low Hardness; Resilient; UV Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Rubber Replacement

RoHS Compliance: RoHS Compliant

Automotive Specifications: CHRYSLER MS-AR-100 IGV Color: Black; FORD Unspecified Color: Black; GM GMN3927 Color: Black; GM GMW15812 P-TPV (EPDM+PP) Type 2 Color: Black; VAG VW82034 Color: Black; VAG VW91101 Color: Black

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ISO 1183
Viscosity 210 cP
@Shear Rate 206 1/s,
Temperature 200 °C
210 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  34
@Time 5.00 sec
34
@Time 0.00139 hour
Extruded; ISO 868
 36
@Time 5.00 sec
36
@Time 0.00139 hour
Injection Molded; ISO 868
Tensile Strength at Break 2.60 MPa377 psiFlow; ISO 37
 3.30 MPa479 psiAcross Flow; ISO 37
 3.14 MPa
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
455 psi
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air at 168 hr; ISO 188
 3.37 MPa
@Treatment Temp. 150 °C,
Time 605000 sec
489 psi
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air at 168 hr; ISO 188
Tensile Stress at Strain  0.800 MPa
@Strain 100 %
116 psi
@Strain 100 %
Across Flow; ISO 37
 1.70 MPa
@Strain 100 %
247 psi
@Strain 100 %
Flow; ISO 37
 0.832 MPa
@Strain 100 %,
Treatment Temp. 135 °C
121 psi
@Strain 100 %,
Treatment Temp. 275 °F
Across Flow, Change in Air at 1000 hr; ISO 188
 1.77 MPa
@Strain 100 %,
Treatment Temp. 150 °C
256 psi
@Strain 100 %,
Treatment Temp. 302 °F
Across Flow, Change in Air at 168 hr; ISO 188
Elongation at Break 210 %210 %Flow; ISO 37
 530 %530 %Across Flow; ISO 37
 594 %
@Treatment Temp. 150 °C,
Time 605000 sec
594 %
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air at 168 hr; ISO 188
 610 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
610 %
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air at 168 hr; ISO 188
Tear Strength 9.99 kN/m57.0 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set  12 %
@Temperature 22.8 °C,
Time 79200 sec
12 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 23 %
@Temperature 70.0 °C,
Time 79200 sec
23 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 42 %
@Temperature 125 °C,
Time 252000 sec
42 %
@Temperature 257 °F,
Time 70.0 hour
ISO 815
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Sarlink® TPV 5790B Thermoplastic Vulcanizate
Stellarchem SV-B65E TPV Compound
RTP Company RTP 2720 S-30A Saturated Styrenic Block Copolymer
Avient Elastamax™ XL 0162-25 EPDM TPV-Based Thermoplastic Elastomer
Avient Elastamax™ XL 0162-28 EPDM TPV-Based Thermoplastic Elastomer

PTEKNQ1208 / 237699

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.