MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay TOLCIDE® PS 70A 70% tetrakis hydroxymethyl phosphonium sulfate
Categories: Other Engineering Material

Material Notes: Identification: CONCENTRATE BASED UPON TETRAKIS(HYDROXYMETHYL)PHOSPHONIUM SULPHATE (THPS) AND A BIOPENETRANT

CAS: 55566-30-8

Function: Concentrate for formulation into TOLCIDE® PS70A, PS50A & PS20A

Foam Potential: Non-foaming

Available in: Asia Pacific, Europe, Latin America and North America

Application: TOLCIDE® PS70A is a rapid acting, powerful microbiocide which has been designed to control bacteria in oilfield water-flood operations and production systems. It can be used to control reservoir souring in oilfields contaminated with sulphate reducing bacteria and alleviate production problems associated with iron sulphide deposition. With a relatively low order of aquatic toxicity and being both biodegradable and nonbioaccumulative, TOLCIDE® PS70A is approved for use in many environmentally sensitive areas of the world including the North Sea. TOLCIDE® PS70A is supplied as a liquid formulation which is non-foaming, fully miscible with water and insoluble in oils.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 - 1.40 g/ccOSTM059
pH 3.0 - 6.0OSTM056
 
Thermal PropertiesOriginal ValueComments
Melting Point <= -15.0 °CFreezing Point
 
Descriptive Properties
AppearancePale yellow to pale pink liquidOSTM078
Assay69-72%OPTI103
Turbidity<15 NTUOSTM064

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WRHOD854 / 138085

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.