MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Röhm PLEXIGLAS® Softlight 7N df23 PMMA
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: PLEXIGLAS® Softlight 7N df23, based on PLEXIGLAS® 7N, is characterized by diffuse scattering of light.

Typical properties of PLEXIGLAS® molding compound are

  • good flow
  • high mechanical strength, surface hardness and mar resistance
  • very good weather resistance
Special properties of PLEXIGLAS® Softlight 7N df23 injection molding items for lighting engineering applications
  • excellent light diffusion combined with excellent light transmittance.
Application: Used for injection molding items for lighting engineering applications

Information provided by Roehm America LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccISO 1183
Melt Flow 4.1 g/10 min
@Load 3.80 kg,
Temperature 230 °C
4.1 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 65.0 MPa9430 psi5 mm/min; ISO 527
Elongation at Break 2.5 %2.5 %5 mm/min; ISO 527
Tensile Modulus 3.40 GPa493 ksi1 mm/min; ISO 527
Charpy Impact Unnotched 1.70 J/cm²8.09 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.180 J/cm²0.857 ft-lb/in²ISO 179/1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.30 µm/m-°C
@Temperature 0.000 - 50.0 °C
3.50 µin/in-°F
@Temperature 32.0 - 122 °F
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 101 °C214 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C207 °FISO 75
Vicat Softening Point 105 °C221 °FB / 50; ISO 306
Glass Transition Temp, Tg 108 °C226 °FISO 11357
Glow Wire Ignition Temperature 700 °C1290 °FIEC 60695-2
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 81 %81 %ISO 13468-2
 
Processing PropertiesMetricEnglishComments
Die Temperature 220 - 260 °C428 - 500 °FExtrusion
Melt Temperature 220 - 260 °C428 - 500 °F
Drying Temperature <= 95.0 °C<= 203 °FPredrying
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourPredrying, Desiccant-Type Drier
 
Descriptive Properties
Half-Value Angle21°DIN 5036

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROHM9364 / 319981

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.