MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nouryon Trigonox BPIC-C75 Polymer tert-Butylperoxy isopropyl carbonate, 75% solution in odorless mineral spirits
Categories: Other Engineering Material

Material Notes: Trigonox BPIC-C75 is an initiator (75% active ingredient in odorless mineral spirits) for (co)polymerization of ethylene, styrene, acrylonitrile, acrylates and methacrylates.

CAS number: 2372-21-6

EINECS/ELINCS No: 219-143-7

Applications: For Polymer Production: Polymerization of styrene: Trigonox BPIC-C75 can be used for the polymerization and copolymerization of styrene in the temperature range of 95-125°C. During polymerization the temperature is increased in steps. For Thermoset: Trigonox BPIC-C75, tert-butylperoxy isopropyl carbonate, is an aliphatic percarbonate, which is used for the curing of unsaturated polyester resins at elevated temperatures. Trigonox BPIC-C75 is especially developed for the curing of UP resin based Hot Press Moulding formulations (SMC, DMC, BMC etc) in the temperature range of 120 - 170°C. Trigonox BPIC-C75 gives a long shelf life stability of the compound. Trigonox BPIC-C75 can in comparison with Trigonox C, tert-butyl peroxybenzoate, be characterized as a faster and more efficient peroxide. This means a faster and more optimal cure with a lower residual styrene content of the moulded part. In combination with an optimal Low Profile or Low Shrink formulation a very smooth and regular surface of the moulded product can be achieved. The decomposition products of Trigonox BPIC-C75 are low volatile compounds, which makes the peroxide very suitable for the production of e.g. microwave cookware.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³
Half-life  0.100
@Temperature 137 °C
0.100
@Temperature 279 °F
[hr]
 1.00
@Temperature 117 °C
1.00
@Temperature 243 °F
[hr]
 10.0
@Temperature 98.0 °C
10.0
@Temperature 208 °F
[hr]
Viscosity 2.3 cP2.3 cP
Molecular Weight 176.2 g/mol176.2 g/mol
Storage Temperature -20.0 - 25.0 °C-4.00 - 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 70.0 °C158 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Assay74.0-76.0 %
Color= 10 Pt-Co / APHA
Content= 0.10 %Hydroperoxides as TBHP
 = 150 mg/kgInorganic + organic hydrolysable chloride
 6.72-6.90 %Active oxygen
Content (%)9.08Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1166 / 286689

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.