MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sika Sikaflex® 110 Liquid Seam Sealant
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Sikaflex 110 Liquid Seam Sealant is a non-shrinking, 100% solids, solvent free polyether based, moisture curing, elastomeric sealant. It forms a weather-tight seal when applied over sheathing board joints. Its distinctive blue color allows easy visual verification that all seams and gaps have been effectively sealed.

Where to Use: For use on exterior gypsum board sheathing, extruded polystyrene, EPS, concrete and plywood construction materials and it is installed prior to applying an air barrier coating.

Advantages:

  • Sealant can be left exposed for up to 6 months
  • The placement of Sikflex 100 Liquid Seam Sealant to seal joints between construction materials is in compliance with the International Energy Conservation Code (IECC) mandatory requirements Section 502.5, 502.4, and 502.4.3 to seal the building envelope for Air Leakage and Moisture Control.

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Solids Content 100 %100 %
Volatile Organic Compounds (VOC) Content 15.7 g/l15.7 g/l
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2727ASTM D2240
Tensile Strength 1.10 MPa160 psiASTM D412/C1135
Tensile Stress at Strain  0.517 MPa
@Strain 50 %
75.0 psi
@Strain 50 %
ASTM C1184
 0.793 MPa
@Strain 100 %
115 psi
@Strain 100 %
ASTM C1184
Elongation at Break 200 %200 %ASTM D412/C1135
Shear Strength 0.965 MPa140 psiASTM C961
Peel Strength 0.657 kN/m3.75 pli100%; ASTM C794
 0.789 kN/m4.50 pli200%; ASTM C794
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature >=15.0 °C
12.0 Month
@Temperature >=59.0 °F
in original unopened cartridge
 
Descriptive Properties
AppearanceLightly textured, distinctive blue color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sika SikaFlex® 201 Adhesive

PSIKA923 / 209830

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.