MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lord Adhesives PC10678 Silver Conductor
Categories: Fluid

Material Notes: LORD PC10678 silver conductor is designed for screen print application onto flexible substrates. It is primarily used in the manufacture of membrane switches and as a highly-conductive grid and busbar for solar cell applications.

Features: primarily intended for use on polyester and polycarbonate surfaces; can also be used on rigid surfaces such as glass and ceramic. provides good rheological properties; may be used in manual and high-speed automatic applications including the roll-to-roll manufacturing process. cured film is abrasion resistant; adhesion is improved through a low temperature drying profile. cured film provides excellent flexibility for use on flexible substrates. cured film provides excellent electrical conductivity.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 3000 - 5000 cP
@Temperature 25.0 °C
3000 - 5000 cP
@Temperature 77.0 °F
Brookfield HBT, Spindle CP-51, 10 rpm
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 25.0 °C
6.00 Month
@Temperature 77.0 °F
from date of manufacture in original, unopened container
 
Descriptive Properties
AppearanceSilver Paste
Resistivity0.04 maxohms/sq/mil, Dried on Mylar at 100 C for 30 min
 0.06 maxCrease Resistivity, ohms/sq/mil, Fold and crease conductive trace interior 180 C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9322 / 232678

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.