MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Process Technologies Inc Viton® Extreme™ Compound 2001 Sanitary Gasket/O-Ring
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Process Technologies Viton® Extreme sanitary gaskets and O-Rings are produced from formulated Viton® Extreme ETP-600S fluoroelastomer. This unique material is produced with Advanced Polymer Architecture. (APA) It represents a proprietary advance in fluoroelastomer technology developed by DuPont Performance Elastomers. Viton Extreme sealing elements exhibit excellent resistance to steam and to attack by an exceptionally broad variety of chemicals and fluids. They can solve the most challenging chemical applications in the pharmaceutical and biotechnology industries. Sterilization processes used by pharmaceutical, biotechnology, food and beverage manufacturers frequently use steam or caustic chemicals or a combination of both. These aggressive conditions put special demands on commonly used sanitary gasket materials such as EPDM, silicone, PTFE and bisphenol-cured FKM. EPDM is capable of providing excellent steam resistance, but exhibits relatively poor resistance to some commonly used cleaning fluids. Seals made with silicone may provide good resistance to a wide variety of cleaning fluids, but have relatively poor steam resistance. PTFE seals offer excellent resistance to steam and chemical attack, but because of their plastic nature, can creep under stress. Bisphenol-cured FKM has good steam resistance but is less resistant to some caustic sterilization processes. Process Technologies offers its Viton Extreme compound 2001 in all sanitary gasket sizes for Tri-Clover® Tri-Clamp®

Information provided by Process Technologies Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75ASTM D2240
Tensile Strength at Break 2315 psiASTM D412
Elongation at Break 198 %ASTM D412
100% Modulus 1.079 ksi
@Strain 100 %
ASTM D412
Compression Set 27 %
@Temperature 200 °C,
Time 252000 sec
25% Deflection, in Air % of original deflection; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -26.0 °C
 
Descriptive Properties
ColorBlack
Compatibility for ChemicalsAcetoneGood
 AmmoniaNot Recommended
 Hydrochloric AcidExcellent
 Hydrofluoric AcidLimited
 Hydrogen PeroxideExcellent
 Isopropyl AlcoholExcellent
 Nitric AcidExcellent
 Phosphoric AcidExcellent
 Sodium HydroxideExcellent
 Sodium HypochloriteExcellent
 Steam to 400ºF (204ºC)Limited
 Sulfuric AcidExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Precision Polymer Engineering E80Q Ethylene Propylene Rubber
Process Technologies Inc Sanifluor® 1000 Formulated Aflas® Elastomer
Greene Tweed FLUORAZ® 890 Fluoroelastomer, FEPM
Fluorseals PTFE Unfilled
Precision Polymer Engineering E85Q Ethylene Propylene Rubber

PPTI03 / 138115

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.