MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Master Bond UV15SP-1 Low Viscosity, UV Curable System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond UV15SP-1 is a new one component, high strength UV curable epoxy resin based polymer system for bonding, sealing, & coating with high performance properties. It is a 100% reactive, low viscosity liquid at ambient temperatures which does not contain any solvents or other volatiles. When exposed to a source of UV light, Master Bond UV15SP-1 produces durable, strong, tough and chemically resistant coatings and adhesive/sealants with excellent electrical insulation properties. Fastest cures are obtained with light sources emitting at a wave length of 250-320 nm. Shrinkage upon cure is less than one-third that of conventional UV systems. The cured coatings and adhesive/sealants can be used over the wide temperature range of -60°F to over 300°F. Unlike many other commercially available UV curable products, Master Bond UV15SP-1 is not oxygen inhibited and exhibits a desirably fast cure rate at ambient temperatures even in the presence of air. The superior performance profile of UV15SP-1 is due to its effective cationic catalyst curing mechanism. Post curing the UV15SP-1 at 90° to 125°C for 30 minutes will give it a glass transition temperature over 125°C, far higher than conventional type UV systems. This post cure is also effective in enhancing chemical resistance, particularly to solvents. Master Bond UV15SP-1 can be cured in very short time periods, e.g. 1 minute and less, at ambient temperatures with various commercial UV lamps. A conventional 200 watt/inch medium pressure mercury lamp is recommended. Even with low intensity UV sources, cures can be obtained quickly. No solvents or other volatiles are released during the curing process. Cured coatings or adhesive/sealants are durable and tough and feature excellent adhesion to both metallic and nonmetallic substrates, from bonderized steel to Mylar polyester film. Impact strengths are high — Gardner impact measurements exceed 320 inch #. Properties of typical UV15SP-1 coatings are summarized in table #1. Storage stability of Master Bond UV15SP-1 is 6 months under the usual storage conditions in unopened containers.

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 100 - 130 cPuncured coating
 
Mechanical PropertiesOriginal ValueComments
Gardner Impact >= 275 in-lbreverse
 >= 320 in-lbface
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.60e+9 ohm-cm
Dielectric Constant 2.96
@Frequency 1e+6 Hz,
Temperature 25.0 °C
 3.14
@Frequency 60 Hz,
Temperature 25.0 °C
 3.52
@Frequency 1e+6 Hz,
Temperature 100 °C
 3.76
@Frequency 1e+6 Hz,
Temperature 150 °C
 3.91
@Frequency 60 Hz,
Temperature 100 °C
 4.85
@Frequency 60 Hz,
Temperature 150 °C
Dissipation Factor 0.0040
@Frequency 1e+6 Hz,
Temperature 25.0 °C
 0.020
@Frequency 60 Hz,
Temperature 25.0 °C
 0.023
@Frequency 60 Hz,
Temperature 150 °C
 0.026
@Frequency 1e+6 Hz,
Temperature 100 °C
 0.030
@Frequency 60 Hz,
Temperature 100 °C
 0.032
@Frequency 1e+6 Hz,
Temperature 150 °C
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point >= 350 °F
Flash Point >= 200 °FCleveland Open Cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.517
 
Descriptive Properties
Acetone double rubs>1001 day
 >1802 hours
Crosshatch Adhesion1
Pencil HardnessH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 3-6371 UV GEL
Dow 3-4170 DIELECTRIC GEL KIT
Momentive Performance Materials RTV102 One Component Acetoxy Adhesive Sealant, White
Momentive Performance Materials IS808 One-Component, Paste Consistency Silicone Rubber Adhesive Sealant, Translucent
Momentive Performance Materials IS802 One-Component, Paste Consistency Silicone Rubber Adhesive Sealant, White

PMASTB365 / 149612

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.